| Title: | Mechanical properties of 5083 aluminium welds after manual and automatic pulsed gas metal arc welding using E5356 filler |
| Authors: | Mutombo, K Du Toit, M |
| Keywords: | Mechanical properties Aluminium welds Aluminium alloy ER5356 filler wire Metals |
| Issue Date: | 2010 |
| Publisher: | Trans Tech Publications |
| Citation: | Mutombo, K and Du Toit, M. 2010. Mechanical properties of 5083 aluminium welds after manual and automatic pulsed gas metal arc welding using E5356 filler. Materials Science Forum, Vol. 654-656, pp 2560-2563 |
| Abstract: | Semi-automatic and automatic pulsed gas metal arc welding (GMAW) of aluminium alloy 5083 with ER5356 filler wire causes considerable softening in the weld. The tensile strength of dressed automatic welds approaches that of the base metal, but the stress concentration caused by the weld toe in undressed semi-automatic welds reduced the tensile strength significantly. Fully automatic welds displayed improved fatigue properties compared to semi-automatic welds. |
| Description: | Copyright: 2010 Trans Tech Publications. This is the authors pre-print version. The definitive version is published in the Materials Science Forum, Vol. 654-656, pp 2560-2563 Paper also presented at the 7th Pacific Rim International Conference on Advanced Materials and Processing (PRICM7), Cairns Convention Centre, Cairns, Australia, 2-6 August 2010 |
| URI: | http://www.scientific.net/MSF.654-656.2560 http://hdl.handle.net/10204/4217 |