The effect of solution treatment on the microstructure and mechanical properties of as-cast Ti-Mo alloys

Show simple item record

dc.contributor.author Moshokoa, Nthabiseng
dc.contributor.author Raganya, Mampai L
dc.contributor.author Obadele, BA
dc.contributor.author Olubambi, PA
dc.contributor.author Machaka, Ronald
dc.date.accessioned 2021-04-23T16:09:16Z
dc.date.available 2021-04-23T16:09:16Z
dc.date.issued 2020
dc.identifier.citation Moshokoa, N., Raganya, M.L., Obadele, B., Olubambi, P. & Machaka, R. 2020. The effect of solution treatment on the microstructure and mechanical properties of as-cast Ti-Mo alloys. <i>Materials Today: Proceedings, 38(2).</i> http://hdl.handle.net/10204/12000 en_ZA
dc.identifier.issn 2214-7853
dc.identifier.uri https://doi.org/10.1016/j.matpr.2020.05.784
dc.identifier.uri http://hdl.handle.net/10204/12000
dc.description.abstract The present study investigates the effect of solution treatment on the microstructure and mechanical properties of as-cast Ti-Mo alloys. The two alloys (Ti-8Mo and Ti-9Mo) were fabricated using a commercially available Arc re-melting furnace. Thereafter, the ingots were subjected to solution treatment and then quenched in ice water. Phase identification, microstructural analysis and fracture surfaces of both the as-cast and solution treated alloys were investigated using the X-ray diffraction (XRD) and Optical microscope (OM). The mechanical properties of both the alloys in the as-cast and solution treated state were characterized using the tensile test to obtain the elastic modulus and 3-point bend test to get the bending properties. The XRD results for Ti-8Mo alloy in as-cast and solution treated condition show dominant a phase peaks and Ti-9Mo alloy in as-cast condition show the dominant ß phase peaks and a phase peaks. However, the XRD showed a phase peaks after solution treatment. The optical micrographs of both alloys in as-cast condition show equi-axed beta grains with sub-grain boundaries within the grains. On the other hand, the Ti-9Mo alloy show needle like structure within the beta equi-axed grains after solution treatment while the Ti-8Mo show only needle like structures without beta equi-axed grains. The fracture surfaces after tensile test in the as-cast condition display cleaved and dimple features of various sizes while the fracture surface of the alloy after solution treatment show only dimple features. The elastic modulus obtained after tensile test decreases after solution treatment. The bending strength of Ti-8Mo alloy decreased after solution treatment whereas the Ti-9Mo alloy show a significant increase in the bending strength after solution treatment. en_US
dc.format Abstract en_US
dc.language.iso en en_US
dc.relation.uri https://www.sciencedirect.com/science/article/pii/S2214785320343972 en_US
dc.source Materials Today: Proceedings, 38(2) en_US
dc.subject Bending strength en_US
dc.subject Elastic modulus en_US
dc.subject Optical microscope en_US
dc.subject Solution treatment en_US
dc.subject Molybdenum equivalence en_US
dc.title The effect of solution treatment on the microstructure and mechanical properties of as-cast Ti-Mo alloys en_US
dc.type Article en_US
dc.description.pages 1054-1058 en_US
dc.description.note Copyright: 2020 Elsevier. This is the abstract version of the work. For access to the fulltext, please visit the publisher's website en_US
dc.description.cluster Manufacturing en_US
dc.description.impactarea Powder Metallurgy Technologies en_US
dc.identifier.apacitation Moshokoa, N., Raganya, M. L., Obadele, B., Olubambi, P., & Machaka, R. (2020). The effect of solution treatment on the microstructure and mechanical properties of as-cast Ti-Mo alloys. <i>Materials Today: Proceedings, 38(2)</i>, http://hdl.handle.net/10204/12000 en_ZA
dc.identifier.chicagocitation Moshokoa, Nthabiseng, Mampai L Raganya, BA Obadele, PA Olubambi, and Ronald Machaka "The effect of solution treatment on the microstructure and mechanical properties of as-cast Ti-Mo alloys." <i>Materials Today: Proceedings, 38(2)</i> (2020) http://hdl.handle.net/10204/12000 en_ZA
dc.identifier.vancouvercitation Moshokoa N, Raganya ML, Obadele B, Olubambi P, Machaka R. The effect of solution treatment on the microstructure and mechanical properties of as-cast Ti-Mo alloys. Materials Today: Proceedings, 38(2). 2020; http://hdl.handle.net/10204/12000. en_ZA
dc.identifier.ris TY - Article AU - Moshokoa, Nthabiseng AU - Raganya, Mampai L AU - Obadele, BA AU - Olubambi, PA AU - Machaka, Ronald AB - The present study investigates the effect of solution treatment on the microstructure and mechanical properties of as-cast Ti-Mo alloys. The two alloys (Ti-8Mo and Ti-9Mo) were fabricated using a commercially available Arc re-melting furnace. Thereafter, the ingots were subjected to solution treatment and then quenched in ice water. Phase identification, microstructural analysis and fracture surfaces of both the as-cast and solution treated alloys were investigated using the X-ray diffraction (XRD) and Optical microscope (OM). The mechanical properties of both the alloys in the as-cast and solution treated state were characterized using the tensile test to obtain the elastic modulus and 3-point bend test to get the bending properties. The XRD results for Ti-8Mo alloy in as-cast and solution treated condition show dominant a phase peaks and Ti-9Mo alloy in as-cast condition show the dominant ß phase peaks and a phase peaks. However, the XRD showed a phase peaks after solution treatment. The optical micrographs of both alloys in as-cast condition show equi-axed beta grains with sub-grain boundaries within the grains. On the other hand, the Ti-9Mo alloy show needle like structure within the beta equi-axed grains after solution treatment while the Ti-8Mo show only needle like structures without beta equi-axed grains. The fracture surfaces after tensile test in the as-cast condition display cleaved and dimple features of various sizes while the fracture surface of the alloy after solution treatment show only dimple features. The elastic modulus obtained after tensile test decreases after solution treatment. The bending strength of Ti-8Mo alloy decreased after solution treatment whereas the Ti-9Mo alloy show a significant increase in the bending strength after solution treatment. DA - 2020 DB - ResearchSpace DP - CSIR J1 - Materials Today: Proceedings, 38(2) KW - Bending strength KW - Elastic modulus KW - Optical microscope KW - Solution treatment KW - Molybdenum equivalence LK - https://researchspace.csir.co.za PY - 2020 SM - 2214-7853 T1 - The effect of solution treatment on the microstructure and mechanical properties of as-cast Ti-Mo alloys TI - The effect of solution treatment on the microstructure and mechanical properties of as-cast Ti-Mo alloys UR - http://hdl.handle.net/10204/12000 ER - en_ZA
dc.identifier.worklist 24452 en_US


Files in this item

This item appears in the following Collection(s)

Show simple item record